1 -- integral bolster, rough forged, in W2 tool steel
2 -- rough ground


3 -- salt pot coming up to temperature (1475 degrees F)
4-- bringing the blade to critical temperature


5 -- out of the salt
6 -- into the quench


7 -- hardened and tempered blade
8 -- finish grinding the hardened blade


9 -- wet finish grinding
10 -- hand-finishing